Just picked up a LEE mold for the 7mm08 C285-130 Looking at the data of the 3 powders I have the most of 4064, 4895, 3031.I'm thinking I'll come up with a load using H4895..........I'll be happy to work up a load for a youngster that is around 2500ft/sec Using WW lead GC'd
Hoping this is a bore rider or at least a snug fit?

Any worry about that short neck and losing a GC in the powder? Or do you just make sure the GCs are snug fit?